Tungsten Powder:
Parameters | Particle Size - Wet Sieve |
Particle size – Fisher Number (FSSS) (µm) |
Chemical analysis |
Hydrogen Loss (%) |
Application | |
<45 µm (%) |
Other metallic impurities (%) |
Tungsten (%) |
||||
|
(ASTM D-185) | (ASTM B-330) | (AAS) | (ASTM E-159) | ||
TUN | 98.5 min | 4 max | 1 max | 97 min | 2 max |
Wet sieving with mineral spirit as rinsing liquid.
AAS-Atomic Absorption Spectrophotometer
Spongy Irregular shape
(Used for Diamond tools, Ferrous & non-ferrous alloys, High speed tool steel, Industrial catalysts, Powder metallurgy parts, Sintering applications, Welding electrodes, x-ray & electron tubes etc.,)