Copper Alloy Powder: (Cu/Sn) Bronze (Pre- Alloyed)-Spherical:
Parameters | Particle Size - Dry Sieve | Chemical analysis | Application | |||
>75 µm (%) |
>45 µm (%) |
<45 µm (%) |
Copper (%) |
Tin (%) |
||
|
(ASTM B-214 ) | (AAS) | ||||
BN 91 SS | 3 max | Balance | 60 - 80 | 88 - 90 | 10 - 11.5 | |
BN 8515 SS | 1 max | Balance | 65 - 85 | 84 - 86 | 14 - 16 | |
BN 82 SS | 3 max | Balance | 65 - 80 | 79 - 81 | 18 - 20 |
The sieve value of each sieve is the retention after passing through its previous sieve.
AAS-Atomic Absorption Spectrophotometer
Air Atomized-Spherical shape
(Used for Abrasives, Adhesives, Automobile parts, Bearings, Brake linings, Chemicals, Diamond tools, oil filters, Plastics, Powder metallurgy parts, Sintering parts, Watch components applications etc., )